International Journal For Multidisciplinary Research
E-ISSN: 2582-2160
•
Impact Factor: 9.24
A Widely Indexed Open Access Peer Reviewed Multidisciplinary Bi-monthly Scholarly International Journal
Home
Research Paper
Submit Research Paper
Publication Guidelines
Publication Charges
Upload Documents
Track Status / Pay Fees / Download Publication Certi.
Editors & Reviewers
View All
Join as a Reviewer
Get Membership Certificate
Current Issue
Publication Archive
Conference
Publishing Conf. with IJFMR
Upcoming Conference(s) ↓
Conferences Published ↓
ISC-AISGF-TBRF
DePaul-2026
IC-AIRCM-T3-2026
NSSFIGTMA-2025
SPHERE-2025
AIMAR-2025
SVGASCA-2025
ICRTET-4
ICCE-2025
Chinai-2023
PIPRDA-2023
ICMRS'23
Contact Us
Plagiarism is checked by the leading plagiarism checker
Call for Paper
Volume 8 Issue 6
November-December 2026
Indexing Partners
Effect of Solidification Kinetics and Vickers Indentation Conditions on Mechanical Properties of Sn-Bi-Cd Alloy
| Author(s) | Rajesh Kant |
|---|---|
| Country | India |
| Abstract | The present work examines the relationship between anisotropic growth velocity and the mechanical behaviour of the Sn–Bi–Cd eutectic composite. The alloy was prepared from the constituent metals using the heat-chill method and its eutectic melting point was determined by differential scanning calorimetry. The composition investigated was Sn 25.9 wt%, Bi 53.9 wt%, Cd 20.2 wt%, with a measured eutectic melting point of 376.2 K. Macrohardness-related strength modes and Vickers microhardness were evaluated as functions of growth velocity, indentation time and applied load. At 3.10 × 10⁻⁷ m s⁻¹, the modulus of rupture is 52.10 × 10⁵ N m⁻², tensile strength is 63.90 × 10⁴ N m⁻² and compressive strength is 66.30 × 10⁴ N m⁻². Microhardness rises from 16.40 kg mm⁻² at 0.50 × 10⁻⁷ m s⁻¹ to 35.30 kg mm⁻² at 3.10 × 10⁻⁷ m s⁻¹ and decreases to 17.10 kg mm⁻² at 7.50 × 10⁻⁷ m s⁻¹. At 20 g, Hv remains approximately 34.50–34.80 kg mm⁻² over 20–150 s. Hv decreases from 36.50 kg mm⁻² at 10 g to 16.70 kg mm⁻² at 100 g. The results demonstrate a characteristic optimum or moderate-growth region in which the fibrous eutectic microstructure and mechanical response are maximized. The observations support the manuscript’s interpretation that directional/fibrillar growth produces stronger, more coherent microstructures than instantaneous or very rapid growth. |
| Keywords | eutectic composite; anisotropic growth; growth velocity; macrohardness; microhardness; Vickers hardness; fibrillar microstructure. |
| Field | Chemistry |
| Published In | Volume 4, Issue 3, May-June 2022 |
| Published On | 2022-05-27 |
Share this

E-ISSN 2582-2160
CrossRef DOI prefix of IJFMR is 10.36948/ijfmr
All research papers published on this website are licensed under Creative Commons Attribution-ShareAlike 4.0 International License, and all rights belong to their respective authors/researchers.
Powered by Sky Research Publication and Journals